首页> 外国专利> MANUFACTURING METHOD OF CELLULOSE FIBER CONTROLLED DEGREE OF CRYSTLLITY ACCORDING TO SOLIDIFICATION RATE AND CELLULOSE FIBER PRODUCED BY USING THE SAME

MANUFACTURING METHOD OF CELLULOSE FIBER CONTROLLED DEGREE OF CRYSTLLITY ACCORDING TO SOLIDIFICATION RATE AND CELLULOSE FIBER PRODUCED BY USING THE SAME

机译:凝固速度与纤维素纤维的结晶度的控制方法及使用该方法制得的纤维素纤维

摘要

The present invention relates to a method for manufacturing cellulose fiber capable of controlling the degree of crystallinity according to a solidification rate and, more particularly, to a method for manufacturing cellulose fiber having a low microstructure owing to a low solidification rate when a cellulose solution is manufactured using an an ionic liquid solvent as a mixed solution for dissolving cellulose. Process yield and efficiency are improved when cellulose fiber is manufactured using a high-concentration spinning solution as the cellulose solution manufactured according to the present invention uses an ionic liquid with high solubility. Also, a method for manufacturing cellulose fiber having a low microstructure owing to a low solidification rate is ensured to be able to adjust the microstructure of fiber by configuring correlation between the solidification rate and the degree of crystallinity.
机译:纤维素纤维的制造方法技术领域本发明涉及一种能够根据凝固速度来控制结晶度的纤维素纤维的制造方法,更具体地,涉及在纤维素溶液为纤维素溶液的情况下由于凝固速度低而具有低组织的纤维素纤维的制造方法。使用离子液体溶剂作为溶解纤维素的混合溶液制备的。当使用高浓度纺丝溶液制造纤维素纤维时,由于根据本发明制造的纤维素溶液使用具有高溶解度的离子液体,因此提高了产率和效率。另外,确保了由于凝固速度低而制造微细结构的纤维素纤维的方法,该方法能够通过设定凝固速度与结晶度的相关性来调整纤维的微结构。

著录项

  • 公开/公告号KR101472094B1

    专利类型

  • 公开/公告日2014-12-15

    原文格式PDF

  • 申请/专利权人 HYOSUNG CORPORATION;

    申请/专利号KR20130157767

  • 发明设计人 CHOI JAE SHIN;KIM CHEOL;

    申请日2013-12-18

  • 分类号D01F2;D01D5/06;

  • 国家 KR

  • 入库时间 2022-08-21 15:01:06

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号