In the general formula Ca 1-xy La x (Sr y ' Ba 1-y' ) y Fe 2n-z Co z , which represents the atomic ratio of the metal elements Ca, La, Sr, Ba, Fe and Co, (0.300, 0.392, 0.308), and the coordinates c: (0.300, 0.300, 0.303) in the triangular coordinates of xy, x, Z, and molar ratios are 0.5? Y'? 1 and 0.2 (0.200, 0.330), coordinates d: (0.400, 0.200, 0.400) Wherein the raw material powder is mixed with the raw material powder so as to satisfy? Z 0.25 and 5.2 n 5.6, a step of calcining the mixed raw material powder, a step of crushing the obtained calcined body, firing comprises a step, and the addition of the mixed raw material powder, or the calcined body to SiO 2 of less than 1.5 mass% to 0.1 mass% in the powder body, and in which the calcined body or the calcined body powder, 0 to 2 mass% in terms of CaO Of CaCO 3 is added.
机译:在通式Ca 1-xy La x (Sr y' Ba 1-y' y Fe 2n-z Co z ,它表示金属元素Ca,La,Sr,Ba,Fe和Co的原子比(0.300 ,0.392、0.308)和xy,x,Z和摩尔比的三角坐标中的坐标c:(0.300,0.300,0.303)为0.5?是啊1和0.2(0.200,0.330),坐标d:(0.400,0.200,0.400)其中,将原料粉末与原料粉末混合以满足? Z <0.25且5.2 <n <5.6时,将混合原料粉末煅烧的工序,将得到的煅烧体粉碎的工序,烧成的工序包括将混合原料粉末或煅烧体添加至SiO的工序。粉末体中的 2 小于1.5质量%至0.1质量%,并且其中煅烧体或煅烧体粉末的CaCO相对于CaCO 3为0至2质量% 已添加。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号