首页> 外国专利> ENVIRONMENT-FRIENDLY GROUT FOR FILLING WATERSIDE STRUCTURE AND GROUTING CONSTRUCTION METHOD OF WATERSIDE STRUCTURE USING SAME

ENVIRONMENT-FRIENDLY GROUT FOR FILLING WATERSIDE STRUCTURE AND GROUTING CONSTRUCTION METHOD OF WATERSIDE STRUCTURE USING SAME

机译:填筑河床结构的环境友好灌浆及使用相同方法的河岸结构灌浆施工方法

摘要

This invention relates to a grouting construction method of a waterside structure, and grout used for the same. The grouting construction method according to the present invention is to prevent water penetration by filling pores inside a waterside structure constructed by piling up. The grouting construction method is forming perforated holes by perforating the waterside structure, and injecting grout containing a cement admixture and a high molecular thickener through the perforated holes. The high molecular thickener is mixed with 60-90 wt% of a chelate resin, 5-20 wt% of water, 0.05-5 wt% of a stabilizer, and 1-30 wt% of a rapid-hardening material, and optionally with 1-5 wt% of a high-range water-reducing agent, 0.1-1 wt% of a preservative and 0.1-1 wt% of an antifoaming agent.;COPYRIGHT KIPO 2015
机译:水侧结构的灌浆施工方法及其灌浆技术领域本发明涉及水侧结构的灌浆施工方法及其灌浆。根据本发明的灌浆施工方法是通过填充通过堆积而建造的水侧结构内部的孔来防止水渗透。该灌浆施工方法是通过在水侧结构上打孔来形成打孔的孔,并通过打孔的孔注入含有水泥掺合料和高分子增稠剂的水泥浆。将高分子增稠剂与60-90 wt%的螯合树脂,5-20 wt%的水,0.05-5 wt%的稳定剂和1-30 wt%的快速硬化材料混合,并可选地与1-5 wt%的高范围减水剂,0.1-1 wt%的防腐剂和0.1-1 wt%的消泡剂。; COPYRIGHT KIPO 2015

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号