首页> 外国专利> A nickel catalyst supported on phosphorus-containing mesoporous alumina xerogel support, preparation method thereof and production method of hydrogen gas by steam reforming of liquefied natural gas using said catalyst

A nickel catalyst supported on phosphorus-containing mesoporous alumina xerogel support, preparation method thereof and production method of hydrogen gas by steam reforming of liquefied natural gas using said catalyst

机译:负载在含磷的介孔氧化铝干凝胶载体上的镍催化剂,其制备方法和使用所述催化剂通过液化天然气的蒸汽重整制氢的方法

摘要

present invention is a porous alumina, including medium controlled by a gel (Xerogel) carrier a supported nickel catalyst, a method of manufacturing the same and relates to a method of producing hydrogen gas by steam reforming of liquid natural gas (LNG) using the catalyst, more particularly, steam reforming of the liquefied natural gas (LNG) is used in the hydrogen gas produced by the reaction, and the porosity of 2 to 50 nm range, alumina being controlled by hyeongtaeyi the nickel with 0.1 to 50% by weight, based on the total catalyst weight supported on a carrier, including a gel, the carrier of a / the atomic ratio of aluminum in the range from 0.01 to 1 medium porosity alumina, including the control, characterized in that a nickel catalyst supported on a gel carrier, and a method of manufacturing the vapor of liquefied natural gas (LNG) using the catalyst It relates to a method of producing hydrogen gas by a reforming reaction. By the introduction of phosphorus according to the present invention can improve the adsorption property of the change in reaction to the interaction force between the nickel and the alumina support, the catalyst for the liquefaction of natural gas by applying the steam reforming reaction of (LNG) high purity hydrogen gas efficiently can be produced. ;
机译:本发明是一种多孔氧化铝,其包括由凝胶(Xerogel)载体控制的介质和负载的镍催化剂,其制造方法,并且涉及通过使用催化剂将液态天然气(LNG)进行蒸汽重整来生产氢气的方法。更具体地说,在反应产生的氢气中使用液化天然气(LNG)的蒸汽重整,其孔隙率在2至50 nm范围内,氧化铝是由亨泰伊以0.1至50重量%的镍来控制的,基于负载在包括凝胶的载体上的催化剂的总重量,载体的铝原子比为0.01至1的中等孔隙度氧化铝,包括对照,其特征在于负载在凝胶上的镍催化剂载体,以及使用催化剂制造液化天然气(LNG)的方法,涉及通过重整反应生产氢气的方法。通过根据本发明的磷的引入,可以通过应用(LNG)的蒸汽重整反应来改善对镍与氧化铝载体之间的相互作用力的反应变化的吸附性能,该催化剂是用于天然气液化的催化剂可以有效地生产高纯度氢气。 ;

著录项

  • 公开/公告号KR1015125050000B1

    专利类型

  • 公开/公告日2015-04-16

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR1020130108834

  • 申请日2013-09-11

  • 分类号B01J23/755;C01B3/26;

  • 国家 KR

  • 入库时间 2022-08-21 14:58:18

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号