porous Li having an average particle size of the present invention 1~30, 4 Ti 5 O 12 cathode active material, the Li 4 Ti 5 O 12 2 to 20 parts by weight of the conductive material of the negative electrode active material 100 parts by weight, said Li 4 Ti 5 O 12 cathode active material glycol of the hydrophobic compound from 0.1 to 10 parts by weight based on 100 parts by weight of the Li 4 Ti 5 O 12 on 100 parts by weight of negative electrode active material About 2 to 20 parts by weight of the binder and the Li 4 Ti 5 O 12 , including the negative electrode active material dispersion medium 100-1200 parts by weight per 100 parts by weight and, wherein the glycol of the hydrophobic compound is ethylene glycol, diethylene glycol, triethylene glycol, propylene glycol, polyethylene glycol and at least one material selected from polypropylene glycol, and the dispersion medium are ethanol, isopropyl alcohol, propanol, It relates to a process for the production of lithium-titanium oxide-based negative electrode using lithium titanium oxide for a negative electrode composition comprising the one or more materials selected from the butanol and water. According to the present invention, the electrode density is improved, and the negative electrode active material and the conductive material in the dispersion is enhanced, it is possible to inhibit the moisture absorption of the electrode itself, water absorption swelling battery or super capacitor is being suppressed swelling (swelling) developing This occurrence can be suppressed to improve the life characteristics. ;
机译:具有本发明的平均粒径的多孔Li 1〜30,4 Ti 5 O 12 正极活性物质,Li 4 Ti 5 O 12 2至20重量份负极活性物质的导电材料100重量份,称Li 4 Ti 5 O 12 疏水化合物的正极活性物质二醇,基于100重量份的Li 4为0.1至10重量份 Ti 5 O 12 在100重量份的负极活性材料上约2至20重量份的粘合剂和Li 4 < / Sub> Ti 5 O 12 ,其中,负极活性物质分散介质相对于100重量份为100〜1200重量份,其中,疏水性化合物的二醇为是乙二醇,二甘醇,三甘醇,丙二醇,聚乙二醇和选自聚丙二醇的至少一种材料,且分散介质为乙醇,异丙醇,丙醇,涉及一种使用锂钛氧化物作为负极组合物的基于锂钛氧化物的负极的制造方法,该负极组合物或从丁醇和水中选择的更多材料。根据本发明,可以提高电极密度,并且可以提高分散液中的负极活性物质和导电性物质,可以抑制电极本身的吸湿,吸水膨胀型电池或超级电容器。抑制膨胀(膨胀)的发展这种现象可以得到抑制,以改善寿命特性。 ;

著录项

  • 公开/公告号KR1015169750000B1

    专利类型

  • 公开/公告日2015-05-04

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR1020130082591

  • 发明设计人 조민영;노광철;박선민;

    申请日2013-07-15

  • 分类号H01M4/485;H01M4/1391;H01M4/62;

  • 国家 KR

  • 入库时间 2022-08-21 14:58:14

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号