The present invention relates to an eco-friendly lightweight aggregate with low carbon using a dry bottom ash by crushing and gravity grinding, and a manufacturing method thereof. More particularly, the eco-friendly lightweight aggregate of the present invention has an excellent aspect ratio of 1 to 2 range by crushing and gravity grinding the bottom ash discharged by air-cooling the same in a heat power plant, satisfies unit volume mass not more than 880 kg/m^3 (coarse aggregate) and not more than 1,120 kg/m^3 (fine aggregate) which are a reference of structural KS lightweight aggregate, has absolute density of 1.3 to 1.8 kg/m^3 and total porosity of 26 to 50 w% which are an equivalent level comparing with an artificial lightweight aggregate circulated in the domestic and foreign countries, has high closed porosity of 13 to 46 w% and low absorptivity of 4 to 10%, which are outstanding levels compared to the artificial lightweight aggregate, and also has rough texture since a small spherical air gap is formed on a surface while a general shape is closer to a spherical shape.
机译:本发明涉及使用通过粉碎和重力磨碎的干底灰的低碳环保轻质骨料及其制造方法。更特别地,本发明的环保轻质骨料通过在火力发电厂中通过对通过空冷而排出的底灰进行粉碎和重力研磨而具有1至2范围的优异的长宽比,满足单位体积质量大于880 kg / m ^ 3(粗骨料)且不超过1,120 kg / m ^ 3(细骨料),是结构性KS轻质骨料的参考,绝对密度为1.3至1.8 kg / m ^ 3,总孔隙率与在国内外流通的人造轻质骨料相比,其含量为26至50 w%的当量水平,具有13至46 w%的高封闭孔隙率和4至10%的低吸收率,与人造轻质骨料,并且由于表面上形成了小的球形气隙,而总体形状更接近球形,因此质地也粗糙。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号