1. A method of creating explosives olfactory simulator (BB) for learning search dogs, comprising applying to the substrate BB samples of the sorption material, characterized in that the sorption material is odorologicheski neutral porous inert material, a fragment of which is placed in a sealed container placed BB sample therein, the container is heated to a temperature not exceeding the melting point BB and incubated for a time sufficient to partially or fully saturate I porous material pairs VV.2. A method according to claim 1, characterized in that as neutral odorologicheski porous inert material is foamed polyethylene foam or foamed penopolipropilen.3. A method according to claim 1, characterized in that the degree of saturation of the porous inert material BB pairs regulate residence time of said material in the sample konteynere.4. A method according to claim 1, characterized in that the degree of saturation of an inert material BB pairs regulate the heating temperature of the sample used VV.5. A method according to claim 1, characterized in that the degree of concentration of explosive vapors of an inert material is controlled by changing the geometric dimensions it poverhnosti.6. A method according to claim 1, characterized in that the fragment of the porous inert material positioned within the container without contact with the bottom, top and side walls konteynera.7. A method according to claim 1, characterized in that the sealed container is made of a material not generating extraneous odors upon heating, such as stainless steel.
机译:1。一种用于学习搜寻犬的炸药嗅觉模拟器(BB)的制造方法,包括将吸附材料的样品施加到基底BB上,其特征在于,吸附材料是odorologicheski中性多孔惰性材料,将其片段放置在吸附剂中。在其中放入BB样品的密封容器中,将容器加热至不超过熔点BB的温度,并温育足以使I个多孔材料对VV.2部分或完全饱和的时间。 2.根据权利要求1所述的方法,其特征在于,作为中性的气味学多孔惰性材料,是泡沫聚乙烯泡沫或泡沫戊三醇。 2.根据权利要求1所述的方法,其特征在于,所述多孔惰性材料BB对的饱和度调节所述材料在样品konteynere中的停留时间。 2.根据权利要求1所述的方法,其特征在于,惰性材料BB对的饱和度调节所使用的样品的加热温度VV.5。 2.根据权利要求1所述的方法,其特征在于,惰性材料的爆炸性蒸气的浓度通过改变其几何尺寸来控制。6。 2.根据权利要求1所述的方法,其特征在于,所述多孔惰性材料的碎片定位在所述容器内,而不与​​底部,顶部和侧壁konteynera.7接触。 2.根据权利要求1所述的方法,其特征在于,所述密封容器由加热时不会产生异味的材料制成,例如不锈钢。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号