METHOD OF OBTAINING FOAM-GENERATOR FOR FOAM-CONCRETE CONSTRUCTIONS

机译:在泡沫混凝土结构中使用泡沫发生器的方法

摘要

FIELD: chemistry.;SUBSTANCE: invention relates to a method of obtaining ampholytic surface-active substances on the basis of a protein-containing raw material and can be used in the process of production of foam-concrete and foam-concrete constructions. In the method of obtaining a foam-generator for the production of foam-concrete and foam-concrete constructions, including the hydrolysis of the protein-containing raw material in the presence of calcium hydroxide, calcium hydroxide is formed, when calcium oxide is introduced in a hydrolysed reaction mixture, the hydrolysis process is carried out in one stage in a reactor-hydrolyser, provided with high-speed stirrer and an external circular loop with a pump for 5-9 hours at a temperature of 110-132°C with the weight ratio of initial ingredients "feather wastes:water:calcium oxide", equal to 100 : (350-400) : (3.5-3.7), with pH of the lime-feather mass at the beginning of hydrolysis varying within the interval of 12.0-12.4, and at the end of hydrolysis in the interval of 7.5-7.7.;EFFECT: obtaining the foam-generator with high foam-generating properties, which are achieved both with the application of moderately mineralised water and alkaline highly hard lime water.;1 ex, 1 tbl
机译:技术领域本发明涉及一种基于含蛋白质的原料获得两性表面活性物质的方法,并且可用于生产泡沫混凝土和泡沫混凝土结构的过程中。在获得用于生产泡沫混凝土和泡沫混凝土结构的泡沫发生器的方法中,包括在氢氧化钙的存在下水解含蛋白质的原料,当向其中引入氧化钙时,形成氢氧化钙。在水解反应混合物中,水解过程是在反应器-水解器中进行的,该反应器-水解器配有高速搅拌器和带泵的外部环形回路,在110-132°C的温度下进行5-9小时。初始成分“羽毛废料:水:氧化钙”的重量比,等于100:(350-400):(3.5-3.7),水解开始时石灰-羽毛块的pH值在12.0的区间内变化-12.4,并且在水解结束时在7.5-7.7之间。效果:获得具有高泡沫生成性能的泡沫发生器,这可以通过应用中等矿化水和碱性高硬石灰水来实现。 ; 1 ex,1 tbl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号