FIELD: technological processes.;SUBSTANCE: invention relates to rolling. Hollow bars are cast by electroslag melting from low plastic steel "04Х14Т5Р2Ф-Ш" with boron content from 2.0 to 3.0% with size of 470±5×vn.270±5×3000±50 mm. They are ground and turned into hollow blooms with size of 455±5×vn.280±5×3000±50 mm. Heated to temperature of 1040-1060°C. Rolled into pig pipe stocks with size of 287×11×25600-29600 mm on burnishers 266/267 with drawing µ from 9.69 to 10.86 and clamping by diameter Δ from 33.5 to 39.1%. Pipe stalks are cut with a hot saw into multiple-length pipes of 10200±50, 11500±100 mm and straightened. Multiple-length pipes are cut into two stock arms with length of at least 5000 mm. They are ground and turned into stock pipes with size of 280.8±2.0×5+1.5/-1.0 mm and profiled into hexahedral pipes of the specified size.;EFFECT: invention provides for reduced metal consumption.;5 cl
机译:技术领域本发明涉及轧制。中空棒是通过电渣从低塑料钢“04Х14Т5Р2Ф-Ш”中熔炼而成的,硼含量为2.0%至3.0%,尺寸为470±5×vn.270±5×3000±50 mm。它们被研磨并变成空心花,尺寸为455±5×vn.280±5×3000±50 mm。加热到1040-1060℃的温度。在266/267抛光机上将其轧制成尺寸为287×11×25600-29600 mm的生猪管坯,拉深µ从9.69到10.86,直径Δ夹紧在33.5到39.1%之间。用热锯将管柄切成10200±50、11500±100 mm的多段管,并拉直。将多长管切成两个库存臂,长度至少为5000 mm。将它们研磨并变成尺寸为280.8±2.0×5 + 1.5 / -1.0 mm的原管,并成型为指定尺寸的六面体管。效果:本发明减少了金属消耗; 5 cl

著录项

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号