首页> 外国专利> METHOD OF PRODUCING COLLOIDAL GEL-LIKE LEAD STYPHNATE

METHOD OF PRODUCING COLLOIDAL GEL-LIKE LEAD STYPHNATE

机译:制备胶体状胶状苯乙烯基硬脂酸酯的方法

摘要

FIELD: chemistry.;SUBSTANCE: synthesis is carried out by uniformly feeding, for 2-2.5 hours, 4% sodium styphnate solution into 15% lead nitrate solution, while keeping temperature of the reaction mixture not higher than 18°C and mixing until formation of a turbulent stream with Reynolds number Re of not less than 200000. The 4% sodium styphnate solution, having pH not lower than 12, is obtained by adding sodium hydroxide with 20% stoichiometric excess to a solution (suspension) of styphnic acid while mixing for 10-20 minutes at 20-25°C. Fixation of the gel-like state of the colloidal lead styphnate is carried out by heating to 40-50°C while mixing for 60 minutes.;EFFECT: obtaining colloidal gel-like lead styphnate as an end product, which retains its properties not only during the precipitation process, but during subsequent storage for not less than 6 months and use in the production of a wide range of primers.
机译:领域:化学;目的:通过将4%的苯甲酸钠溶液均匀地加入15%的硝酸铅溶液中2-2.5小时,同时保持反应混合物的温度不高于18°C并混合直至形成来进行合成的雷诺数Re不小于200000的湍流。通过将20%化学计量过量的氢氧化钠添加到苯甲酸的溶液(悬浮液)中,同时获得pH值不小于12的4%苯甲酸钠溶液。在20-25°C下放置10-20分钟。通过加热至40-50°C并混合60分钟来固定胶体状苯乙烯甲酸酯的凝胶状状态;效果:获得最终产物的胶体状凝胶状苯乙烯甲酸酯铅,不仅保留了其特性在沉淀过程中,但在随后的储存中不少于6个月,并用于生产各种引物。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号