首页> 外国专利> CATHODE ACTIVE MATERIAL FOR NONAQUEOUS SECONDARY BATTERY, MANUFACTURING METHOD THEREOF, CATHODE FOR NONAQUEOUS SECONDARY BATTERY, NONAQUEOUS SECONDARY BATTERY AND ON-VEHICLE NONAQUEOUS SECONDARY BATTERY MODULE

CATHODE ACTIVE MATERIAL FOR NONAQUEOUS SECONDARY BATTERY, MANUFACTURING METHOD THEREOF, CATHODE FOR NONAQUEOUS SECONDARY BATTERY, NONAQUEOUS SECONDARY BATTERY AND ON-VEHICLE NONAQUEOUS SECONDARY BATTERY MODULE

机译:非水二次电池的阴极活性材料,其制造方法,非水二次电池的阴极,非水二次电池和车载非水二次电池模块

摘要

PROBLEM TO BE SOLVED: To provide a cathode active material for nonaqueous secondary battery capable of obtaining high capacity at an atmospheric temperature by suppressing cycle deterioration, a nonaqueous secondary battery and on-vehicle nonaqueous secondary battery module.SOLUTION: The cathode active material for nonaqueous secondary battery comprises an internal part 1, an intermediate part 2 which is provided on a surface of the internal part, and a surface part 3 which is provided on a surface of the intermediate part. The surface part 3, the intermediate part 2 and the internal part have different compositions, contain Ni and Mn, comprise a layered structure and include particles for which an atomic concentration Cs of Ni in the surface part 3, an atomic concentration Cm of Ni in the intermediate part 2 and an atomic concentration Cc of Ni in the internal part satisfy the relation of CsCmCc and a concentration gradient Gs of the atomic concentration of Ni in the surface part 3 and a concentration gradient Gm of the atomic concentration of Ni in the intermediate part 2 satisfy the relation of GsGm.SELECTED DRAWING: Figure 1
机译:解决的问题:提供一种非水系二次电池用正极活性物质,非水系二次电池和车载用非水系二次电池组件。二次电池包括内部部分1,设置在内部部分的表面上的中间部分2和设置在中间部分的表面上的表面部分3。表面部分3,中间部分2和内部部分具有不同的成分,包含Ni和Mn,构成层状结构,并且包括表面部分3中Ni的原子浓度Cs,Ni的原子浓度Cm的颗粒。中间部分2和内部的Ni的原子浓度Cc满足Cs <Cm <Cc与表面部分3中的Ni的原子浓度的浓度梯度Gs和N的原子浓度的浓度梯度Gm的关系。中间部分2中的Ni满足Gs

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有