COMPOSITION FOR (METH)ACRYLIC RESIN CAST PLATE, (METH)ACRYLIC RESIN CAST PLATE PRODUCED BY CAST-POLYMERIZING THE COMPOSITION AND METHOD FOR PRODUCING (METH)ACRYLIC RESIN CAST PLATE BY CAST-POLYMERIZING THE COMPOSITION

机译:(甲基)丙烯酸树脂浇铸板的组成,由(Cast-Polymerize)组合物生产的(甲基)丙烯酸树脂浇铸板和通过将其浇铸聚合的方法(甲基)丙烯酸树脂浇铸板的方法

摘要

PROBLEM TO BE SOLVED: To provide a composition that can produce a (meth)acrylic resin cast plate having excellent heat resistance while maintaining transparency and having good impact resistance while retaining a high elastic modulus, to provide a (meth)acrylic resin cast plate produced by cast-polymerizing the composition and to provide a method for producing a (meth)acrylic resin cast plate by cast-polymerizing the composition.SOLUTION: The (meth)acrylic resin cast plate is produced by cast-polymerizing a composition having the following composition: the composition for a (meth)acrylic resin cast plate containing 1 to 99 mass% of (A) a mono(meth)acrylate, 99 to 1 mass% of (B) a di(meth)acrylate represented by formula (1) as given below, and 0.05 to 2 pts.mass, based on 100 pts.mass of the total of the mono(meth)acrylate (A) and the di(meth)acrylate (B), of (C) a thermoplastic polymer as given below. Formula (1) is CH=CR-COO-(X)-COCR=CH(provided that (X) has a number average molecular weight of 500 or more and is at least one kind of residue selected from CHO, CHO and CHO; and Rrepresents H or CH). The thermoplastic polymer (C) is a thermoplastic polymer comprising 50 to 100 mass% of a methyl metacrylate and 0 to 50 mass% of at least one kind of other vinyl monomers copolymerizable therewith and having a mass average molecular weight of 500,000 to 5,000,000.
机译:解决的问题:提供一种组合物,该组合物可以生产具有优异的耐热性同时保持透明性并且具有良好的耐冲击性同时保持高弹性模量的(甲基)丙烯酸树脂铸板,从而提供一种生产的(甲基)丙烯酸树脂铸板。通过浇铸聚合该组合物并提供通过浇铸聚合该组合物来生产(甲基)丙烯酸树脂浇铸板的方法。解决方案:(甲基)丙烯酸树脂浇铸板是通过浇铸聚合具有以下组成的组合物生产的:(甲基)丙烯酸树脂铸板用组合物,其包含(A)1〜99质量%的单(甲基)丙烯酸酯,(B)99〜1质量%的式(1)表示的二(甲基)丙烯酸酯。 (C)热塑性聚合物的单(甲基)丙烯酸酯(A)和二(甲基)丙烯酸酯(B)的总量的100点质量,如下文所述,以及0.05至2点质量。如下。式(1)为CH = CR-COO-(X)-COCR = CH(式(1),其数均分子量为500以上,且为选自CHO,CHO和CHO中的至少一种残基。 R代表H或CH)。热塑性聚合物(C)是包含50至100质量%的甲基丙烯酸甲酯和0至50质量%的至少一种可与其共聚的且平均分子量为500,000至5,000,000的其他乙烯基单体的热塑性聚合物。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号