INJECTION MATERIAL FOR SEMIFLEXIBLE PAVING AND SEMIFLEXIBLE PAVING

机译:半柔性路面和半柔性路面的注射材料

摘要

PROBLEM TO BE SOLVED: To provide an injection material for semiflexible paving having excellent freeze-thaw resistance as well as excellent in development of initial strength and a semiflexible paving using the injection material.SOLUTION: There are provided an injection material forming a semiflexible paving with compressive strength of material age after injection of 2 hours of 5 N/mmor more, having cement amount of 55 wt.% or more, containing a fine aggregate, a rapid hardening material, a powder resin, a water-reducing agent, and an AE agent, and having water powder ratio of cement milk of 42 wt.% or less, viscosity of cement milk of 250 to 500 mPa s, and air amount of 2 to 12 vol.%, preferably water powder ratio of 39 wt.% or less, viscosity of cement milk of 290 to 360 mPa s, and air amount of 5.3 to 9.0 vol.%, and a semiflexible paving formed by the injection material.SELECTED DRAWING: Figure 1
机译:解决的问题:提供一种用于半柔性铺路的注射材料,该材料具有优异的抗冻融性,并且具有优异的初始强度发展性,并且使用该注射材料进行半柔性铺路。水泥含量为55 wt。%或以上的2小时注射后5小时(5 N / mm)或更多的材料时效抗压强度,其中包含细骨料,快速硬化材料,粉末树脂,减水剂和AE剂,水泥乳的水粉比例为42重量%以下,水泥乳的粘度为250〜500mPa·s,空气量为2〜12体积%,优选水粉比例为39重量%。或更低,水泥乳的粘度为290至360 mPa s,空气量为5.3至9.0 vol。%,由注射材料形成的半柔性铺面。图1

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号