POWDER COMPACT CORE, MANUFACTURING METHOD THEREOF, ELECTRONIC/ELECTRIC PART HAVING POWDER COMPACT CORE, AND ELECTRONIC/ELECTRIC DEVICE WITH ELECTRONIC/ELECTRIC PART MOUNTED THEREON
POWDER COMPACT CORE, MANUFACTURING METHOD THEREOF, ELECTRONIC/ELECTRIC PART HAVING POWDER COMPACT CORE, AND ELECTRONIC/ELECTRIC DEVICE WITH ELECTRONIC/ELECTRIC PART MOUNTED THEREON
PROBLEM TO BE SOLVED: To provide a powder compact core including powder of crystalline magnetic material and powder of amorphous magnetic material, and having a superior magnetic property even in a high-frequency band of 1 MHz or higher.SOLUTION: Powder compact core comprises: powder of crystalline material magnetic material; and powder of amorphous magnetic material. When the dependence of an iron loss Pcv (unit: kW/m) measured under the condition that effective maximum magnetic flux density Bis 15 mT on a frequency f(unit: kHz) is represented by the formula (1) below by use of two constants kand k, one constant kis equal to or less than 1.5×10kW/m/kHz/(mT), and the other constant kis equal to or less than 3.0×10kW/m/(kHz)/(mT): Pcv=k×f×B+k×f×B(1).
展开▼
机译:要解决的问题:提供一种压粉铁心,其包括晶体磁性材料的粉末和非晶态磁性材料的粉末,并且即使在1 MHz或更高的高频下也具有优异的磁性能。解决方案:压粉铁心包括:晶体材料磁性材料的粉末;和无定形磁性材料的粉末。当在有效最大磁通密度Bis 15 mT对频率f(单位:kHz)的条件下测得的铁损Pcv(单位:kW / m)时,用下式(2)表示常数kand k,一个常数kis等于或小于1.5×10kW / m / kHz /(mT),另一个常数kis等于或小于3.0×10kW / m /(kHz)/(mT):Pcv = k×f×B + k×f×B(1)。
展开▼