摘要

The chabazite-type zeolite of the present invention has a SiO 2 /Al 2 O 3 molar ratio of less than 15, and an average particle size from 1.0 µm to 8.0 µm. The chabazite-type zeolite of the present invention has excellent durability and heat resistance, and the copper- loaded chabazite-type zeolite has an improved NOx reduction rate at low temperatures compared to conventional copper- loaded chabazite-type zeolite.
机译:本发明的菱沸石型沸石的SiO 2 / Al 2 O 3摩尔比小于15,平均粒径为1.0μm〜8.0μm。本发明的菱沸石型沸石具有优异的耐久性和耐热性,并且与常规的铜负载菱沸石型沸石相比,负载铜的菱沸石型沸石在低温下具有提高的NOx还原率。

著录项

  • 公开/公告号JP5895510B2

    专利类型

  • 公开/公告日2016-03-30

    原文格式PDF

  • 申请/专利权人 東ソー株式会社;

    申请/专利号JP20110279974

  • 发明设计人 有賀 耕;青山 英和;伊藤 悠軌;

    申请日2011-12-21

  • 分类号C01B39/48;B01D53/94;B01J29/76;B01J32;

  • 国家 JP

  • 入库时间 2022-08-21 14:40:13

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号