The invention relates to the production of materials which can be used in lubricating compositions for treating friction assemblies and also for restoring the friction surfaces of mechanism and machine parts. The composition is produced from the products of dehydration of natural and/or synthesized hydrates and/or mixtures thereof at an inherent water removal temperature and dehydration product stabilization temperature of 300-1200°C. The composition contains oxides from the series MgO and/or SiO 2 and/or Al 2 O 3 and/or CaO and/or Fe 2 O 3 and/or K 2 O and/or Na 2 O and is a garnet-shaped conglomerate consisting of a nanograin and an amorphous binding phase. The size of the conglomerate is in a range of 100-100000 nm and the size of the nanograin is in a range of 2-2000 nm. The claimed method includes a step for stabilizing the dehydration product at a temperature of 900-1200°C for a period of 1-3 hours, which makes it possible to form a stable conglomerate structure.
机译:本发明涉及可用于润滑组合物的材料的生产,所述润滑组合物用于处理摩擦组件并且还用于恢复机构和机器部件的摩擦表面。该组合物由天然和/或合成的水合物和/或其混合物在固有的脱水温度和脱水产物稳定温度为300-1200℃下的脱水产物制成。该组合物包含来自MgO和/或SiO 2和/或Al 2 O 3和/或CaO和/或Fe 2 O 3和/或K 2 O和/或Na 2 O系列的氧化物,并且是石榴石状的团块。由纳米颗粒和无定形结合相组成。团块的尺寸在100-100000nm的范围内,并且纳米颗粒的尺寸在2-2000nm的范围内。所要求保护的方法包括将脱水产物在900-1200℃的温度下稳定1-3小时的步骤,这使得可以形成稳定的聚集体结构。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号