MULTICOMPONENT SYSTEM FOR PRODUCTION OF THERMOPLASTIC-RUBBER COMPOSITE MOULDINGS AND METHOD FOR PREPARING SAID MOULDINGS

机译:用于生产热塑性塑料复合成型品的多组分系统和制备所述成型品的方法

摘要

Multicomponent system for production of thermoplastic-rubber composite mouldings comprising 1) a thermoplastic component and 2) a rubber component comprising a) one or more elastomers, where those elastomers of which 30% by weight or more are present in the rubber component, based on 100% by weight as the entirety of all of the elastomers of the rubber component, must be peroxidically vulcanizable, and b) two or more peroxidic crosslinking agents, where at least one peroxidic crosslinking agent whose decomposition temperature T1/2 (lh) is in the range from 70 to 130°C and at least one second peroxidic crosslinking agent whose decomposition temperature T1/2 (lh) is in the range from 120 to 160°C is used, where at least two peroxidic crosslinking agents are present whose difference in decomposition temperature T1/2 (lh) is at least 5°Cwhere the one or more thermoplastics present in the thermoplastic component 1) have been selected from the group consisting of one of more polyamides, polyimides, polyethers, polyesters, polyphenylene sulphide (PPS), polycarbonates-and combinations thereof.
机译:用于生产热塑性橡胶复合模制品的多组分体系,其包含1)热塑性组分和2)橡胶组分,其包含a)一种或多种弹性体,其中基于橡胶组分的重量计30%或更多的那些弹性体橡胶组分所有弹性体的全部重量的100%必须是可过氧化硫化的,并且b)两种或多种过氧化物交联剂,其中至少一种过氧化物交联剂的分解温度T1 / 2(lh)为在70至130℃的范围内,使用至少一种第二过氧化物交联剂,其分解温度T1 / 2(1h)在120至160℃的范围内,其中存在至少两种过氧化物交联剂,它们之间的差异为分解温度T1 / 2(lh)至少为5°C,其中热塑性组分1)中存在的一种或多种热塑性塑料选自以下一种或多种聚酰胺:酰亚胺,聚醚,聚酯,聚苯硫醚(PPS),聚碳酸酯及其组合。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号