the object of the application is the way of low carbon u017celazokrzemochromu electric furnaces u0142ukowo - resistance heated.process for the production of low carbon u017celazokrzemochromu electric furnaces u0142ukowo - resistance heated by conducting redukcyjnej in atmosphere, in the presence of carbon, the smelting raw mix, consisting of wysokowu0119glowego ferro chromium przeru00f3bczego and kwarcytu,periodic trigger liquid u017celazokrzemochromu vats trigger and giving him a refining process in the refining, characterised by the fact that at the time of the trigger into the vat and vat to refining, to smooth u017celazokrzemochromu introduces silica dust originating from pro cesu purification of gases from furnaces for the production of silicon alloys.silica dust contains at least 92% by weight of amorphous silica, having strong binding properties of silicon carbide, sic and forming on the surface of the liquid metal, a layer of slag on the properties of application of thermal blankets, which during at least 120 minutes utrzymyw ana is the temperature in the liquid u017celazokrzemochromu, preferably 1500 - 1400u00b0c.the dust grains are spherical silica with a specific surface area, preferably from 15 to 35 m2 / g, whose size is not greater than 0045 mm, and the apparent density of dust shall not exceed 250 kg / m3.
机译:本申请的目的是通过在大气中,在有碳存在的情况下在环境中进行redukcyjnej加热来制造低碳电阻的低碳方法。冶炼原料混合物,包括wysokow铬铁przer kwarcytu和周期性的触发液,在精炼过程中会触发提炼过程,其特征在于在触发时进入提桶和提桶为了提纯,使表面光滑,硅粉尘源于从生产硅合金的炉子中净化气体的过程中产生的硅粉尘。硅粉尘中至少含有92%重量比的无定形硅石,具有很强的碳化硅,碳化硅和成型性。在液态金属表面上,一层矿渣的应用性能毛毯,至少在120分钟内是液体中的温度,优选1500-1400°C。尺寸不大于0045毫米,灰尘的表观密度不得超过250千克/立方米。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号