Mother mix for use in a process of preparing a composite material, the mother mixture comprising a mixture of a first amorphous polymer with carbon nanotubes, at least 5%, and preferably 5% to 15% by weight of nanotubes of carbon based on the total weight of the mother mix as determined in accordance with ISO 11358, and having a high load fluidity index HLMI1 of less than 40 g / 10 min determined at 200 ° C under a load of 21.6 kg according to ISO1133, the mother mix characterized in that the first amorphous polymer has an MFI1 flow rate of at least 10 g / 10 min determined at 200 ° C under a load of 5 kg according to ISO1133H.
展开▼
机译:用于制备复合材料的母混合物,该母混合物包含第一无定形聚合物与碳纳米管的混合物,基于总碳纳米管的重量计至少5%,优选5%至15%根据ISO 11358确定的母混合物的重量,并根据ISO1133在200°C和21.6 kg的载荷下测定的高负荷流动性指数HLMI1小于40 g / 10 min第一无定形聚合物的MFI1流速至少为10 g / 10 min,根据ISO1133H在200℃,5 kg载荷下测定。