首页> 外国专利> METHOD FOR PREPARING URANIUM CONCENTRATES BY FLUIDISED BED PRECIPITATION, AND PREPARATION OF UO3 AND U3O8 BY DRYING/CALCINING SAID CONCENTRATES

METHOD FOR PREPARING URANIUM CONCENTRATES BY FLUIDISED BED PRECIPITATION, AND PREPARATION OF UO3 AND U3O8 BY DRYING/CALCINING SAID CONCENTRATES

机译:流化床沉淀法制备铀精矿的方法及干燥/煅烧浓缩精矿制备UO3和U3O8的方法

摘要

process for preparing a concentrate of uranium in the form of particlessolids by precipitation from a solutionsoon, with the help of a precipitating agent in a reactor (1).(7) comprising a base, a top partpower plant (2) and an upper part (3), and a lower part (6).solid particles of uranium concentrate to form a bed.under the action of a fluid flowing in the fluid power(7) to the top of the reactor (1) throughin the lower part (6), the central part (2) and the partmore than (3) of the reactor (1) and which is created bythe introduction to the base (7) of the reactor (1) for a fluid recycling(11) from a first level (a)the upper part (3) of the reactor and returned to base without being settled(7) of the reactor (1), an excess of liquid was alsoevacuated through an overflow (10) located at a second level.(b) fixed in the upper part of the reactor; and (3)a process in which the upper end (c) of a fluidized bed of particlessolids is controlled so as to be at a levellower than the first and second levels determined.
机译:制备颗粒形式的铀精矿的方法从溶液中沉淀出来的固体很快,借助反应器中的沉淀剂(1)。(7)包括底座,顶部动力装置(2)和上部(3)以及下部(6)。铀的固体颗粒浓缩形成床。在流体动力的作用下流动(7)穿过反应器(1)的顶部在下部(6),中央部分(2)和该部分超过(3)的反应堆(1),并且由引入反应器(1)的底部(7)以进行流体循环(11)从第一级(a)反应器的上部(3)并在未沉降的情况下返回基座(7)在反应器(1)中,也有过量的液体通过位于第二层的溢流口(10)抽空。(b)固定在反应堆的上部;和(3)颗粒流化床上端(c)的过程固体被控制在一定水平低于确定的第一和第二级别。

著录项

  • 公开/公告号CA2742732C

    专利类型

  • 公开/公告日2016-05-03

    原文格式PDF

  • 申请/专利权人 AREVA NC;

    申请/专利号CA20082742732

  • 申请日2008-11-07

  • 分类号C01G43/00;C01G43/01;

  • 国家 CA

  • 入库时间 2022-08-21 14:21:50