GC technology was used to study escaping fluorine in calcined process of mixed rare earth concentrate. The mixed rare earth concentrate and it adding assistant of CaO-NaCl-CaCl2 were calcined at 400~750 ℃ for 30~120 min, and then total amount of fluorine, exhausting ratio of fluorine, decomposition ratio and the component were determined. The results showed that adding CaO-NaCl-CaCl2 the decomposition ratio was up to 90% at 700 ℃ in 1 h, and the escaping ratio of fluorine decreased from 29.52% to 0.948%. The average inhabitation ratio was 98.39%. This method supplied basis for low energy and clean decomposition of mixed rare earth concentrate.