The present invention relates to a method for manufacturing Eu^(2+)-activated inorganic red phosphor, where the phosphor exhibits an emission spectrum resolvable into a first Gaussian emission curve and a second Gaussian emission curve; the first Gaussian emission curve has a first Gaussian emission curve peak P_1; the first Gaussian emission peak P_1 has peak 1 height H_(P1), peak 1 peak wavelength P[λ]_(P1), and peak 1 area A_(P1); the second Gaussian emission curve has a second Gaussian emission peak P_2; the second Gaussian emission peak P_2 has peak 2 height H_(P2), peak 2 peak wavelength P[λ]_(P2), peak 2 full width at half max FWHM_(P2), and peak 2 area A_(P2); P[λ]P1P[λ]P2 is satisfied; and the peak 2 full width at half max FWHM_(P2) is minimized.;COPYRIGHT KIPO 2016
机译:本发明涉及Eu ^(2+)活化的无机红色荧光粉的制造方法,该荧光粉具有可分解为第一高斯发射曲线和第二高斯发射曲线的发射光谱。第一高斯发射曲线具有第一高斯发射曲线峰值P_1。第一高斯发射峰P_1具有峰1的高度H_(P1),峰1的峰波长Pλ_(P1)和峰1的面积A_(P1);第二高斯发射曲线具有第二高斯发射峰P_2。第二高斯发射峰P_2具有峰2的高度H_(P2),峰2的峰波长Pλ_(P2),峰2的半峰全宽FWHM_(P2)和峰2的面积A_(P2)。满足P P1 <P P2。 ;并且最大半峰FWHM_(P2)处的峰2全宽最小化。; COPYRIGHT KIPO 2016

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号