Of lead, cobalt, potassium, and which does not contain none, high Curie temperature, mechanical quality factor and the piezoelectric provide good piezoelectric ceramic. Therefore the formula 1 in by indicated that the perovskite-type metal oxide, CuO, and MgO to be contained to the piezoelectric ceramic, and wherein the perovskite-type metal oxide 1 mol in respect of CuO content of 0.1 mol% at least 1 mol% or less and , MgO and the content is more than 0.1 mol% to 2 mol% or less it provides a piezoelectric ceramic. Formula 1 (Na x Ba 1-y) (Nb 1-y Ti y) O 3 (wherein 0.85 ≤ x ≤ 0.92, 0.85 ≤ y ≤ 0.92, 0.95 ≤ x / y ≤ 1.05 indicates a.) ;
机译:铅,钴,钾以及其中的任何一种都不含有铅,居里温度高,机械品质因数和压电性均提供良好的压电陶瓷。因此,式1 in表示压电陶瓷中包含钙钛矿型金属氧化物,CuO和MgO,并且其中相对于CuO含量为0.1mol%的1摩尔钙钛矿型金属氧化物至少为1mol。 MgO的含量大于或等于0.1mol%且MgO的含量大于或等于0.1mol%且小于或等于2mol%,则提供了压电陶瓷。 <公式1>(Na x Ba 1-y) (Nb 1-y Ti y) O 3 (其中0.85≤x≤0.92,0.85≤y≤0.92,0.95≤x / y≤1.05表示一种。) ;

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号