CERAMIC COATING AGENT HAVING ECO-FRIENDLY AND ENERGY SAVING CHARACTERISTICS

机译:兼具节能环保特性的陶瓷涂料

摘要

The present invention relates to a ceramic coating agent having eco-friendly and energy-saving characteristics. The ceramic coating agent comprises: a composition (A) including 20-80 parts by weight of silica (SiO_2), 3-15 parts by weight of alumina (Al_2O_3), 2-10 parts by weight of an ingredient selected from the group consisting of zirconia (ZrO_2), titania (TiO_2), yttria (Yi_2O_3) and a mixture thereof, and 0.1-3 parts by weight of a silicone oil polymer based on 100 parts by weight of a solvent; and a composition (B) including 20-60 parts by weight of glycidoxy propyl tri-methoxy silane (GPTMS) based on 100 parts by weight of methyl tri-methoxy silane (MTMS). The ceramic coating agent is obtained by mixing 60-140 parts by weight of the composition (B) based on 100 parts by weight of the composition (A), and carrying out pre-aging at a temperature of 15-25°C for 10-50 hours.;COPYRIGHT KIPO 2016
机译:本发明涉及一种具有环保和节能特性的陶瓷涂层剂。该陶瓷涂层剂包括:组合物(A),其包含20-80重量份的二氧化硅(SiO_2),3-15重量份的氧化铝(Al_2O_3),2-10重量份的选自以下的成分:相对于100重量份的溶剂,氧化锆(ZrO_2),二氧化钛(TiO_2),氧化钇(Yi_2O_3)及其混合物,以及0.1-3重量份的硅油聚合物;组合物(B),基于100重量份的甲基三甲氧基硅烷(MTMS),其包含20-60重量份的环氧丙氧基丙基三甲氧基硅烷(GPTMS)。相对于100重量份的组合物(A),混合60-140重量份的组合物(B),并在15-25℃的温度下进行10小时的预时效处理,从而得到陶瓷涂布剂。 -50小时。; COPYRIGHT KIPO 2016

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号