the present invention, the grain boundary ( ) through the rare earth-rich phase (rich ) when used as a base material of the diffusion method, R H is easy to spread, either substrate that the coercive force ( ) of its own to be a challenge to provide a method of manufacturing the high NdFeB sintered magnet. Hydrogen crushing process to produce the one trillion minutes by roughly crushing the NdFeB-based alloy ingot by having to occlude hydrogen in the NdFeB-based alloy ingot (step S1), and the fine pulverization to produce a fine powder by further grinding the one trillion minutes (step S2) and a charging step for charging the fine powder to the charging vessel (step S3) and, the orientation step of orienting while charging the fine powder to the charging vessel (step S4), and a fine powder after the orientation step charge to the charge container while the sintering process of sintering has the (step S5), not all perform the dehydrogenation heating and vacuum for leaving a, the hydrogen-absorption in the hydrogen crushing process, for each process to the alignment process from the hydrogen crushing process, the hydrogen crushing process carried out by the sintering process under oxygen-free atmosphere from. ;
机译:在本发明中,通过晶界()通过富稀土相(rich)作为基础材料的扩散方法时,R H 易于扩散,无论是底材即矫顽力()本身是提供制造高NdFeB烧结磁体的方法的挑战。通过将NdFeB基合金铸锭中的氢吸留而粗碎NdFeB基合金铸锭,进行氢破碎过程以生产1万亿分钟(步骤S1),并通过进一步研磨1万亿吨进行细粉碎以生产细粉1分钟(步骤S2)和将细粉填充到装料容器中的装料步骤(步骤S3),以及在将细粉填充到装料容器中的同时进行定向的定向步骤(步骤S4),以及定向之后的细粉。从步骤S5到步骤S5,向烧结容器中的分步装料到装料容器中(步骤S5),并不是每个步骤都进行脱氢加热和真空以在氢压碎过程中留下氢吸收过程中的氢吸收。氢破碎过程,氢破碎过程是通过烧结过程在无氧气氛下进行的。 ;

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号