The present invention relates to a manufacturing method for a high efficiency copper oxide-based high efficiency selective absorber plate manufactured by a chemical oxidation technique. The present invention is to manufacture a relatively even absorber plate even if the absorber plate has a complex surface, by manufacturing the absorber plate by the chemical oxidation technique. According to an embodiment of the present invention, the manufacturing method for a high efficiency copper oxide-based high efficiency selective absorber plate manufactured by the chemical oxidation technique comprises: a step of forming a nanoscale structure by the chemical oxidation technique on a copper surface; a step of forming the nanoscale structure including a step of cleaning an organic matter on the copper surface, a step of removing oxide from the copper surface in which the organic matter is cleaned, and a step of chemically oxidizing the surface of the copper in which the oxide is removed using an alkali solution in which sodium hypochlorous acid (NaClO_2), sodium hydroxide (NaOH), sodium fluorophosphoric acid (Na_3PO_4), and DI water are mixed at a predetermined ratio.;COPYRIGHT KIPO 2016
机译:本发明涉及通过化学氧化技术制造的基于高效氧化铜的高效选择性吸收板的制造方法。通过利用化学氧化技术制造吸收板,即使吸收板具有复杂的表面,本发明也能够制造相对均匀的吸收板。根据本发明的实施方式,通过化学氧化技术制造的基于高效氧化铜的高效选择性吸收板的制造方法包括:通过化学氧化技术在铜表面上形成纳米级结构的步骤;形成纳米级结构的步骤包括:在铜表面上清洁有机物的步骤;从其中清洁了有机物的铜表面去除氧化物的步骤;以及化学氧化其中的铜表面的步骤。使用碱溶液去除氧化物,其中将次氯酸钠(NaClO_2),氢氧化钠(NaOH),氟磷酸钠(Na_3PO_4)和去离子水以预定比例混合。; COPYRIGHT KIPO 2016

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号