The present invention relates to a non-tempered steel composition containing carbon (C), silicon (Si), manganese (Mn), sulfur (S), vanadium (V), titanium (Ti), nitrogen (N) And more particularly, to a method of manufacturing a connecting rod including a connecting rod and a connecting rod manufactured using the same and a heat treatment technique for improving the yield strength and fatigue strength of the connecting rod. More specifically, (Si) of 0.80 to 1.20 wt%, manganese (Mn) of 0.80 to 1.20 wt%, sulfur (S) of 0.06 to 0.10 wt%, vanadium (V) of 0.20 to 0.35 wt%, titanium (Ti) And the balance of iron (Fe) and unavoidable impurities, the shank portion, which is a portion where the produced connecting rod is concentrated, has a bainite structure and a machinability of 0.001 to 0.02 wt% The large and small end portions required are formed of a mixed structure of pearlite structure and ferrite, so that yield strength and fatigue strength It relates to a vaginal composition and non-adjustable connecting rod and a method using the same that can improve.
机译:非调质钢组合物技术领域本发明涉及一种非调质钢组合物,其包含碳(C),硅(Si),锰(Mn),硫(S),钒(V),钛(Ti),氮(N),尤其是,本发明涉及一种制造包括连杆和使用该连杆制造的连杆的连杆的方法以及一种用于提高连杆的屈服强度和疲劳强度的热处理技术。更具体地,(Si)为0.80至1.20 wt%,锰(Mn)为0.80至1.20 wt%,硫(S)为0.06至0.10 wt%,钒(V)为0.20至0.35 wt%,钛(Ti)并且,在铁(Fe)和不可避免的杂质的余量中,作为所制造的连杆集中的部分的柄部具有贝氏体组织,切削加工性为0.001〜0.02重量%。形成了所需的大小端部。珠光体组织和铁素体的混合组织的屈服强度和疲劳强度的测定方法本发明涉及一种阴道用组合物和不可调节的连杆及其使用方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号