首页> 外国专利> -- Heat-resistant iron-chromium-aluminium alloy with low chromium vaporization rate and elevated thermal stability

-- Heat-resistant iron-chromium-aluminium alloy with low chromium vaporization rate and elevated thermal stability

机译:-耐热铁铬铝合金,铬汽化率低,热稳定性高

摘要

2.0 to 4.5% of Al, 12-25% Cr, 1.0 to 4% W, 0.25 to 2.0% of Nb, 0.05 to 1.2% of Si, 0.01 to 0.70% Mn, 0.001 to 0.030% of C, 0.0001 to 0.05% Mg, 0.0001 to 0.03% Ca, 0.001 to less than 0.030% P, Up to 0.03% N, Up to 0.01% of S, The remaining Fe, and An iron-chromium-aluminum alloy containing conventional melt-related impurities (in mass%) and having improved heat resistance, low chromium vaporization rate, and good processability.
机译:铝2.0至4.5%,铬12至25%,钨1.0至4%,铌0.25至2.0%,硅0.05至1.2%,锰0.01至0.70%,碳0.001至0.030%,0.0001至0.05% Mg,0.0001至0.03%Ca,0.001至小于0.030%P,N至0.03%N,S至0.01%S,剩余的Fe和含有常规熔融相关杂质的铁铬铝合金(质量%)并具有改善的耐热性,低的铬汽化速率和良好的加工性。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号