首页> 外国专利> FLUX-CORED WIRE FOR GAS-SHIELDED ARC WELDING METHOD FOR WELDING STEEL FOR VERY LOW TEMPERATURE USE AND METHOD FOR MANUFACTURING WELD JOINT

FLUX-CORED WIRE FOR GAS-SHIELDED ARC WELDING METHOD FOR WELDING STEEL FOR VERY LOW TEMPERATURE USE AND METHOD FOR MANUFACTURING WELD JOINT

机译:极低温用焊接钢的气保护弧焊用药芯焊丝及其制造方法

摘要

A problem to be solved by the present invention is to provide a flux-containing wire which can obtain a weld metal having excellent low-temperature toughness and which has a high welding efficiency, and which can eliminate or simplify preheating for suppressing low-temperature cracking.The flux built-in wire is made of CaF2, BaF2, SrF2, MgF2 And LiF, and when the sum of the contents is , the is 2.0 to 7.0% by mass with respect to the total mass of the flux-containing wire, and the content of the Ti oxide, Si oxide, Mg oxide, Al oxide, Zr oxide, and Ca oxide, and when the total content thereof is defined as , The Is in the range of 0.2 to 0.9% by mass with respect to the total mass of the flux-%, And the CaF RTI ID = 0.0 2Is 0.90 or more, and the ratio of To the Is 3.0 or more and 15.0 or less.;
机译:本发明要解决的问题是提供一种含助焊剂的焊丝,该焊剂可以得到具有优异的低温韧性并且具有高焊接效率的焊接金属,并且可以消除或简化用于抑制低温裂纹的预热。助焊剂内置线由CaF 2 ,BaF 2 ,SrF <​​Sub> 2 ,MgF 2 和LiF,且其含量的总和为,相对于含助焊剂的金属丝的总质量为2.0至7.0质量%,并且Ti氧化物,Si氧化物,Mg氧化物,Al氧化物,Zr的含量为氧化物和Ca氧化物,并且当其总含量定义为时,相对于助熔剂%的总质量,Is在0.2至0.9质量%的范围内,并且CaF <0.0。 Sub> 2 为0.90以上,且与The的比率为3.0以上且15.0以下。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号