首页> 外国专利> How to prepare a composition for BAZALTOFIBROARMIROVANNYH DISPERSNOARMIROVANNOGO FOAM

How to prepare a composition for BAZALTOFIBROARMIROVANNYH DISPERSNOARMIROVANNOGO FOAM

机译:如何制备巴扎菲非罗非鱼分散体泡沫的组合物

摘要

A method for preparing bazaltofibroarmirovannyh compositions for dispersion-reinforced foam, comprising preparing a mixture of cement, quartz sand, component particulate reinforcement - basalt fiber and aqueous foaming solution, characterized in that it has three stages, the first - the preparation of cement-sand mixture in a cyclic mixer gravity second - regrinding wet cement-sand mixture in the disintegrator, the third - the turbulent mixing in a mixer with a mixing speed of 500-600 rev / min, wet house Olot cement-sand mixture for no more than 1.0 minutes, with the blowing agent until the desired final density values ​​of mixture of fiber and basalt fiber of no more than 1.0 minutes.
机译:一种制备用于分散体增强泡沫的巴扎特尔布罗夫米罗维尼组合物的方法,其包括制备水泥,石英砂,组分颗粒增强剂-玄武岩纤维和发泡水溶液的混合物,其特征在于它具有三个阶段,第一个阶段是水泥砂的制备。循环混合机中的混合物重力-其次是在粉碎机中再研磨湿的水泥-沙子混合物,第三次-在混合器中以500-600转/分钟的混合速度进行湍流混合,湿房Olot水泥-沙子混合物的混合速度不超过1.0分钟后,用发泡剂直至纤维和玄武岩纤维的混合物的最终最终密度值不超过1.0分钟。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号