FIELD: mining industry.;SUBSTANCE: invention relates to beneficiation of minerals, and more specifically to extraction of nonferrous and noble metals from tailings of planning sulphide ores and their beneficiation products. Method of conditioning cyanide-containing products prior to floatation extraction of nonferrous and noble metals comprises conditioning and flotation of valuable components. Conditioning cyanide-containing products is carried out using aldehydes or ketones, preferably formaldehyde. Treatment with aldehydes or ketones, preferably, formaldehyde, can be carried out in a wide range of pH (1.8-13.0) and temperature (5-70 °C). Duration of treatment with aldehydes or ketones, preferably, formaldehyde, must not be less than 5 seconds. Consumption of aldehyde or ketone, preferably, formaldehyde, depends on composition of liquid phase.;EFFECT: technical result is increased extraction of nonferrous and noble metals, as well as reduced content of free cyanide.;4 cl, 2 tbl
机译:矿物的选矿技术领域本发明涉及矿物的选矿,并且更具体地涉及从计划的硫化矿石及其选矿产品的尾矿中提取有色金属和贵金属。在浮选有色金属和贵金属之前,对含氰化物的产品进行预处理的方法包括对有价值的成分进行预处理和浮选。使用醛或酮,优选甲醛进行调理含氰化物的产物。可以在很宽的pH(1.8-13.0)和温度(5-70°C)范围内用醛或酮(优选甲醛)进行处理。用醛或酮(最好是甲醛)处理的时间不得少于5秒。醛或酮(优选甲醛)的消耗量取决于液相的组成。效果:技术成果是增加了有色金属和贵金属的提取,并减少了游离氰化物的含量。4cl,2 tbl

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号