FIELD: chemistry.;SUBSTANCE: method for obtaining strontium fluoride powder, activated with neodymium fluoride, includes interaction of ammonium fluoride solution with solution, which contains strontium nitrate and neodymium nitrate. Obtained sediment is separated, washed, dried and subjected to thermal processing. Solution, which contains ions of strontium and neodymium with their molar ratio from 0.997:0.003 to 0.98:0.02, respectively, is applied. Ammonium fluoride is taken with 100-120% excess from stoichiometry. Thermal processing of dried sediment is carried out in two stages. First stage is carried out at temperature 200-250°C for 0.5-1 hour at rate of heating 5-7 degree/min, second - at 550-600°C, with rate of heating being 10-15 degree/min in atmosphere of emitted hydrogen fluoride for 2-3 hours.;EFFECT: invention makes it possible to obtain finely disperse water-free powder of strontium fluoride, activated with neodymium fluoride, with homogenous chemical and phase composition and high product output.;9 dwg, 3 tbl, 6 ex
机译:领域:化学。物质:用氟化钕活化的氟化锶粉末的制备方法包括氟化铵溶液与溶液的相互作用,该溶液含有硝酸锶和硝酸钕。将获得的沉淀物分离,洗涤,干燥并进行热处理。使用溶液,该溶液包含锶和钕的离子,其摩尔比分别为0.997:0.003至0.98:0.02。氟化铵的化学计量过量为100-120%。干燥沉积物的热处理分两个阶段进行。第一阶段以5-7度/分钟的加热速率在200-250°C的温度下进行0.5-1小时,第二阶段-550-600°C在大气中以10-15度/分钟的速率进行排放氟化氢2-3小时。效果:本发明可以得到精细分散的无水氟化锶粉末,该氟化锶活化了氟化钕,具有均匀的化学和相组成以及高产量的产品; 9 dwg,3 tbl,6前

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号