THERMOPLASTIC RESIN COMPOSITION FOR REDUCING CREAK AND CREAK REDUCTION STRUCTURE

机译:热塑性塑料树脂组合物用于减少裂纹和减少裂纹的结构

摘要

PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition capable of providing a structure extremely reducing creak generated when components are rubbed each other, maintaining creak reduction effects even when standing it under high temperature for long time and further excellent in impact resistance and molding appearance.SOLUTION: A thermoplastic resin composition [X] for reducing creak contains a rubber reinforced vinyl resin [A] obtained by polymerizing a vinyl monomer [b1] in presence of an ethylene α-olefin rubbery polymer [a1] having Tm (melting point) of 0°C or more and a silicone oil, and has Mooey viscosity (ML1+4, 100°C; according to JIS K6300) of the ethylene α-olefin rubbery polymer [a1] having Tm (melting point) of 0°C or more of 5 to 80. The silicon content derived from the silicone oil in the thermoplastic resin composition [X] is 0.15 mass% or less based on 100 mass% of the thermoplastic resin composition [X].SELECTED DRAWING: None
机译:要解决的问题:提供一种热塑性树脂组合物,该组合物能够提供一种结构,该结构能够极大地减少当组件相互摩擦时产生的吱吱声,即使在高温下长时间放置也可以保持减少龟裂的效果,并且还具有优异的耐冲击性和成型外观解决方案:用于减少吱吱声的热塑性树脂组合物[X]包含橡胶增强乙烯基树脂[A],该树脂通过在具有Tm(熔点)的乙烯α-烯烃橡胶状聚合物[a1]存在下聚合乙烯基单体[b1]而获得。 Tm(熔点)为0℃的乙烯α-烯烃橡胶状聚合物[a1]的Mooey粘度(ML1 + 4,100℃;根据JIS K6300)为0℃以上。 5〜80以上。热塑性树脂组合物[X]中的源自硅油的硅含量相对于热塑性树脂组合物[X] 100质量%为0.15质量%以下。

著录项

  • 公开/公告号JP2017020050A

    专利类型

  • 公开/公告日2017-01-26

    原文格式PDF

  • 申请/专利权人 TECHNO POLYMER CO LTD;

    申请/专利号JP20160206735

  • 发明设计人 MOCHIZUKI ISAMU;EGAWA KAZUYA;

    申请日2016-10-21

  • 分类号C08L51/04;C08L83/04;B60R7/04;B60R13/02;C08F255/02;

  • 国家 JP

  • 入库时间 2022-08-21 14:01:12

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号