PROBLEM TO BE SOLVED: To provide a peel ply capable of sufficient functioning together with a composite substrate derived from different resins without remaining residual fibers after peeling and containing resin in rich.SOLUTION: There is provided peel ply 11 for surface preparation of a composite substrate 10, which contains woven fabric 11a impregnated by a curable resin matrix 11b containing an epoxydized novolac resin, diglycidyl ether of polyphenol, triglycidyl ether of aminophenol, a curing agent and an inorganic filler particle and having resin content of at least 20 wt.%, wherein yarn of the woven fabric 11a has longitudinal direction tensile strength≥70 lbf/in, lateral direction tensile strength≥40 lbf/in, longitudinal direction linear mass density in a range of 50 to 25 denier and lateral direction linear mass density in a range of 50 to 250 denier.SELECTED DRAWING: Figure 1
机译:解决的问题:提供一种剥离层,该剥离层能够与衍生自不同树脂的复合基材一起充分发挥功能,并且剥离后不残留残余纤维,并且树脂含量丰富。解决方案:提供了剥离层11,用于复合基材的表面制备10,其包含浸渍有可固化树脂基体11b的织物11a,所述可固化树脂基体11b包含环氧酚醛清漆树脂,多酚的二缩水甘油醚,氨基酚的三缩水甘油醚,固化剂和无机填料颗粒,并且树脂含量为至少20重量%,其中,织造织物11a的纱线的纵向拉伸强度≥70lbf / in,横向拉伸强度≥40lbf / in,纵向线性质量密度在50至25旦尼尔的范围内,并且横向线性质量密度在50至250旦尼尔。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号