PROBLEM TO BE SOLVED: To provide ecocement which is excellent in easy firing properties, and has a short setting time while securing flowability, and to provide an ecocement clinker capable of producing an ecocement composition and a method for producing the same.SOLUTION: An ecocement clinker contains 0.2-0.8 mass% of NiO. The ecocement clinker can be produced by internally adding 0.2-0.8 mass% of NiO to an ecocement raw material, mixing the substance and then firing the substance.SELECTED DRAWING: None
机译:解决的问题:提供一种具有优异的易烧性并且在确保流动性的同时具有短凝结时间的生态水泥,并提供一种能够生产生态水泥组合物的生态水泥熟料及其制造方法。熟料包含0.2-0.8质量%的NiO。可以通过向生态水泥原料内部添加0.2-0.8质量%的NiO,混合该物质然后煅烧该物质来生产生态水泥熟料。

著录项

  • 公开/公告号JP2017154921A

    专利类型

  • 公开/公告日2017-09-07

    原文格式PDF

  • 申请/专利权人 TAIHEIYO CEMENT CORP;

    申请/专利号JP20160038941

  • 申请日2016-03-01

  • 分类号C04B7/24;C04B7/38;C04B7/36;

  • 国家 JP