The present invention relates to a method of manufacturing a ceramic article (3) from a metal or metal matrix composite preform (1) provided by 3D-printing or by 3D-weaving. The preform (1) is placed in a heating chamber (2), and a predetermined time-temperature profile is applied in order to controllably react the preform (1) with a gas introduced into the heating chamber (2). The metal, the gas and the time-temperature profile are chosen so as to induce a metal-gas reaction resulting in at least a part of the preform (1) transforming into a ceramic. Preferred embodiments of the invention comprises a first oxidation stage involving a metal-gas reaction in order to form a supporting oxide layer (5) at the surface of the metal, followed by a second stage in which the heating chamber (2) is heated to a temperature above the melting point of the metal to increase the kinetics of the chemical reaction. The invention also relates to a number of advantageous uses of a ceramic article manufactured as described.
机译:用3D打印或3D编织提供的金属或金属基质复合预成型件( 1 )制造陶瓷制品( 3 )的方法。将预成型坯( 1 )放置在加热室( 2 )中,并施加预定的时间-温度曲线,以可控制地反应预成型坯( 1 ),并将气体引入加热室( 2 )。选择金属,气体和时间-温度曲线,以引起金属-气体反应,从而导致至少一部分预成型坯( 1 )转变为陶瓷。本发明的优选实施方案包括第一氧化阶段,该第一氧化阶段包括金属-气体反应以在金属表面形成支撑氧化物层( 5 ),随后是第二阶段,其中加热室( 2 )被加热到高于金属熔点的温度,以增加化学反应的动力学。本发明还涉及如上所述制造的陶瓷制品的许多有利用途。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号