首页>
外国专利>
Methods for the production of Potassium sulphate from Potassium containing Minerals at high temperatures
Methods for the production of Potassium sulphate from Potassium containing Minerals at high temperatures
展开▼
机译:在高温下由含钾矿物生产硫酸钾的方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
The method of producing potassium sulfate. These methods include linking water components containing potassium and sulfate to magnesium chloride (mgc23222),thus obtaining a composition comprising cainite; optionally concentrating the kinite of the composition; reaction of the cainite with magnesium sulfate (MgSO₄) and potassium sulfate (K₂SO₄) so as to convert the cainite into leonite (K₂SO₄.MgSO₄.4H₂O);Optionally, connect the lion with water to remove excessive MgSO4; connect the lion with water to soak mgso832424,contained in the leonite and at least substantially precipitate potassium sulfate (K₂SO₄). The method according to the present can be operated at higher temperatures, in particular at temperatures above 35 ° C and does not require a cooling stage of 20 to 25 ° C. The method produces potassium sulfate with a low amount of chloride.
展开▼
机译:生产硫酸钾的方法。这些方法包括将含有钾和硫酸盐的水成分与氯化镁(mgc23222)连接,从而获得包含钙铝石的组合物;任选地浓缩组合物的纽结;使钙铝石与硫酸镁(MgSO 4)和硫酸钾(K 2 SO 4)反应,从而将钙铝石转化为莱昂石(K 2 SO 3 .MgSO 4 .4H 2 O);可选地,将狮子与水连接以除去过量的MgSO 4。将狮子与水连接以浸泡在leonite中并至少基本上沉淀出硫酸钾(K 2 SO 4)的mgso832424。根据本发明的方法可以在较高的温度下,特别是在高于35℃的温度下操作,并且不需要20至25℃的冷却阶段。该方法产生具有少量氯化物的硫酸钾。
展开▼