Provided are: a fiber-reinforced composite material which has mode I interlaminar fracture toughness, mode II interlaminar fracture toughness and compressive strength under heat and humidity conditions at the same time; an epoxy resin composition for obtaining the fiber-reinforced composite material; and a prepreg which is obtained using the epoxy resin composition. An epoxy resin composition for fiber-reinforced composite materials, which contains at least the following constituent elements (A), (B), (C) and(D). (A) An epoxy resin (B) Resin particles that satisfy the following conditions (bl)-(b3) and are insoluble in an epoxy resin (b1) The particle size distribution index is 1.0-1.8. (b2) The particle sphericity is 90 or more. (b3) The glass transition temperature of the particles is 80-180°C. (C) At least one elastomer component that is selected from among block copolymers containing a block having a glass transition temperature of 20°C or less and rubber particles (D) An epoxy resin curing agent
机译:提供:一种纤维增强的复合材料,其在热和湿条件下同时具有I型层间断裂韧性,II型层间断裂韧性和抗压强度;用于获得纤维增强复合材料的环氧树脂组合物;使用该环氧树脂组合物得到的预浸料。用于纤维增强复合材料的环氧树脂组合物,其至少包含以下组成元素(A),(B),(C)和(D)。 (A)环氧树脂(B)满足以下条件(b1)-(b3)并且不溶于环氧树脂(b1)的树脂颗粒。粒径分布指数为1.0-1.8。 (b2)粒子的球形度为90以上。 (b3)颗粒的玻璃化转变温度为80-180℃。 (C)选自包含玻璃化转变温度为20℃以下的嵌段和橡胶颗粒的嵌段共聚物中的至少一种弹性体成分。(D)环氧树脂固化剂

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号