composite material based on diamond is characterized by the fact that phase binding is dwuborek titanium tib1 in quantities of from 5% to 30% by weight.method of manufacturing composite based diamond is that as a binding phase is used mikroproszek dwuborku titanium tib2 in quantities of from 5% to 30% by weight and the mixture output is spiekaniu wysokociu015bnieniowemu under pressure from 7.0 gpa to 9.0 gpa at 1950 k to 2250 k.
机译:基于金刚石的复合材料的特征在于,相结合是重量百分比为5%至30%的dwuborek钛tib1。制造基于复合材料的金刚石的方法是,作为粘结相使用mikroproszek dwuborku钛tib2的数量为重量为5%至30%,混合物的产量为1950 k至2250 k,压力为7.0 gpa至9.0 gpa时的spiekaniu wysokoci u015bnieniowemu。