首页> 外国专利> PROCESS FOR PREPARING MATERIALS IN CHALCOGENIDE SYSTEMS ASS-EUSAND ASS-ERS

PROCESS FOR PREPARING MATERIALS IN CHALCOGENIDE SYSTEMS ASS-EUSAND ASS-ERS

机译:硫属化物系统ASS-EUSAND ASS-ERS中材料的制备过程

摘要

The invention relates to a process for preparing materials in chalcogenide systems AsS-EuSand AsS-ErSwith a view to using them as targets for thin layer deposition using the PLD method and for producing, in the electronics industry, devices emitting in the visible or infrared range , as well as for converting energy from the IR range into the VIS range. According to the invention, the process consists in preparing Asby co-precipitation in the Euand Ersynthesis stage, at the temperature of 80°C, washing the resulting precipitate with deionized water up to a neutral pH value, drying the same in an oven, at 100°C, for 24 h, and, after obtaining the precipitate powders, pouring them into quartz vials having an internal diameter of 14 mm which are introduced into a pure spectral graphite susceptor boat of in inductive heating installation for a heat treatment of the powders at a temperature of 491°C, for 192 min, in a 99.999%-pure Ar-controlled atmosphere, at a pressure of 1.1 atm.
机译:本发明涉及一种在硫族化物系统AsS-EuS和AsS-ErS中制备材料的方法,以期将它们用作通过PLD方法进行薄层沉积的靶,并用于在电子工业中生产在可见或红外范围内发射的器件。 ,以及将能量从IR范围转换为VIS范围。根据本发明,该方法包括在Euand Ersynthesis阶段中,在80℃的温度下制备Asby共沉淀,用去离子水洗涤所得的沉淀物直至中性pH值,在烘箱中将其干燥。在100°C下放置24小时,在获得沉淀物粉末后,将其倒入内径为14 mm的石英瓶中,然后将其引入感应加热设备的纯光谱石墨基座舟皿中,以对粉末进行热处理在纯度为99.999%的Ar控制气氛中,压力为1.1个大气压下,在491°C的温度下持续192分钟。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号