首页> 外国专利> ORE FINE AGGLOMERATE TO BE USED IN SINTERING PROCESS AND PRODUCTION PROCESS OF ORE FINES AGGLOMERATE

ORE FINE AGGLOMERATE TO BE USED IN SINTERING PROCESS AND PRODUCTION PROCESS OF ORE FINES AGGLOMERATE

机译:细粉团矿的烧结工艺和生产过程中使用的细粉团矿

摘要

Discloses a feldspar aggregate to be used in a sintering process wherein the feldspar aggregate is formed by a mixture of feldspar particles and flocculants wherein the particles have a diameter of from 0.01 mm to 8.0 mm. The process of producing minute aggregate of aggregates comprises the steps of using volcanic rock particles having a particle size of less than 0.150 mm; Mixing the colloidal particles with a flocculant at a ratio of about 0.5 to about 5.0 mass percent sodium silicate; Forming wet particles having a diameter of from about 0.01 mm to about 8.0 mm upon addition of water; And drying the wet particles at a temperature varying from about 100 캜 to about 150 캜 to form dry particles resistant to mechanical effort and urea.
机译:公开了一种在烧结过程中使用的长石骨料,其中所述长石骨料由长石颗粒和絮凝剂的混合物形成,其中所述颗粒的直径为0.01mm至8.0mm。生产骨料的细骨料的方法包括使用粒度小于0.150mm的火山岩颗粒的步骤;以约0.5至约5.0质量%的硅酸钠的比例将胶体颗粒与絮凝剂混合;加水后形成直径约0.01mm至约8.0mm的湿颗粒;然后在约100到约150캜的温度下干燥湿颗粒,以形成耐机械力和抗尿素的干颗粒。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号