FIELD: metallurgy.;SUBSTANCE: steel contains, wt %: C: not more than 0.050, Si: 0.01-1.00, Mn: 1.75-2.50, P: not more than 0.050, S: not more than 0.010, Ni: 20.00-24.00, Cr: 23.00-27.00, Mo: 1.80-3.20, N: 0.110-0.180, the rest - Fe and unavoidable impurities. Steel grain size number determined according to JIS G0551 (2005) is at least 6.0, part of area occupied by phase σ does not exceed 0.1%, fluidity point at 230°C is at least 220 MPa, and a corrosion rate in the corrosion test to 65% nitric acid according to JIS G0573 (1999) does not exceed 0.085 g/m2/H.;EFFECT: steel has high temperature strength and corrosion resistance in nitric acid.;2 cl, 2 dwg, 1 tbl, 1 ex
机译:领域:冶金;物质:钢所含,wt%:C:不大于0.050,Si:0.01-1.00,Mn:1.75-2.50,P:不大于0.050,S:不大于0.010,Ni:20.00- 24.00,Cr:23.00-27.00,Mo:1.80-3.20,N:0.110-0.180,其余-Fe和不可避免的杂质。根据JIS G0551(2005)确定的钢晶粒度数至少为6.0,相σ所占的部分面积不超过0.1%,在230℃下的流动点至少为220 MPa,并且在腐蚀试验中的腐蚀速率JIS G0573(1999)中硝酸含量不超过65%的情况下不超过0.085 g / m 2 / H .;效果:钢在硝酸中具有高温强度和耐腐蚀性。; 2 cl,2 dwg,1 tbl,1 ex

著录项

  • 公开/公告号RU2618021C1

    专利类型

  • 公开/公告日2017-05-02

    原文格式PDF

  • 申请/专利权人 NIPPON STIL END SUMITOMO METAL KORPOREJSHN;

    申请/专利号RU20150152343

  • 发明设计人 UEYAMA MASAKI;

    申请日2012-06-20

  • 分类号C22C38/58;

  • 国家 RU

  • 入库时间 2022-08-21 13:23:36

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号