[Abstract] Provided is a method for producing a high-purity tungsten powder having a phosphorus content of less than 1 wtppm; wherein an ammonium tungstate solution containing 1 wtppm or more of phosphorus as an impurity in terms of the inclusion in tungsten is used as a starting material, this solution is neutralized with hydrochloric acid at a temperature of 50°C or less to adjust the pH at 4 or more and less than 7 so as to precipitate ammonium paratungstate undecahydrate crystals, the resulting solution is heated to 70 to 90°C and filtered in a high-temperature state so as to obtain ammonium paratungstate pentahydrate crystals, the obtained crystals are calcined so as to form a tungsten oxide, and the tungsten oxide is subject to hydrogen reduction so as to obtain a high-purity tungsten powder. Additionally provided is a method for producing a high-purity tungsten powder having a phosphorus content of 0.4 wtppm or less; wherein the ammonium tungstate solution is neutralized with hydrochloric acid to adjust the pH at 4 or more and 6 or less, and this solution is subject to the same procedure as described above so as to obtain a high-purity tungsten powder. Consequently, the phosphorus content can be efficiently reduced.
机译:[摘要]提供了一种生产磷含量小于1 wtppm的高纯度钨粉的方法。其中以钨中的夹杂物计,含有1重量ppm以上的磷作为杂质的钨酸铵溶液用作原料,在50℃以下的温度下用盐酸中和该溶液以调节pH。在4以上且小于7的范围内析出仲钨酸铵十一水合物晶体,将得到的溶液加热至70〜90℃,在高温状态下过滤,从而得到仲钨酸五水铵晶体,将其煅烧。然后,将其氧化形成氢氧化钨,然后将其还原以得到高纯度的钨粉。另外提供了一种生产磷含量为0.4wtppm或更少的高纯度钨粉的方法。其中用盐酸中和钨酸铵溶液以将pH调节至4或更高至6或更低,并且对该溶液进行如上所述的相同步骤,以获得高纯度钨粉。因此,可以有效地降低磷含量。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号