摘要

PROBLEM TO BE SOLVED: To provide a heat resistant chlorine-containing crosslinked resin molded body which has excellent appearance and exhibits excellent heat resistance and a method for producing the same, a silane masterbatch and a mixture thereof which can form the heat resistant chlorine-containing crosslinked resin molded body, and a heat resistant product.SOLUTION: There are provided a method for producing a heat resistant chlorine-containing crosslinked resin molded body which includes: a step (a) of melting and mixing an organic peroxide, an inorganic filler and a silane coupling agent with a specific ratio in a base resin containing chlorinated polyethylene and polyvinyl chloride at a temperature equal to or higher than a decomposition temperature of the organic peroxide; a step (b) of mixing silane masterbatch obtained in the step (a) and a silanol condensation catalyst, and then molding the mixed substance; and a step (c) of bringing the molded body obtained in the step (b) into contact with moisture to crosslink, where in the step (a), a ratio of a content of the chlorinated polyethylene and the polyvinyl chloride in the base resin used at the time of the reaction with the silane coupling agent is 90:10 to 10:90 by a mass ratio; a heat resistant chlorine-containing crosslinked resin molded body produced by the same; a silane masterbatch and a mixture thereof; and a heat resistant product.SELECTED DRAWING: None
机译:解决的问题:提供具有优异的外观并且显示出优异的耐热性的耐热性含氯交联树脂成型体及其制造方法,硅烷母料及其混合物,其可以形成耐热性含氯的树脂。解决方案:提供了一种制备耐热的含氯的交联树脂成型体的方法,该方法包括:(a)将有机过氧化物,无机填料熔融并混合的步骤。在等于或高于有机过氧化物的分解温度的温度下,在包含氯化聚乙烯和聚氯乙烯的基础树脂中具有特定比例的硅烷偶联剂;步骤(b):将步骤(a)中获得的硅烷母料与硅烷醇缩合催化剂混合,然后模制混合物质;步骤(c)是使步骤(b)中得到的成型体与水分接触而交联的工序,其中,步骤(a)中,基础树脂中的氯化聚乙烯和聚氯乙烯的含量之比。与硅烷偶联剂反应时使用的质量比为90:10〜10:90。通过该方法制造的耐热性含氯交联树脂成型体。硅烷母料及其混合物;和耐热产品。

著录项

  • 公开/公告号JP2018162424A

    专利类型

  • 公开/公告日2018-10-18

    原文格式PDF

  • 申请/专利权人 FURUKAWA ELECTRIC CO LTD:THE;

    申请/专利号JP20170061905

  • 申请日2017-03-27

  • 分类号C08J3/24;C08L23/28;C08L27/06;C08K5/14;C08K3/00;C08K5/54;C08K5/10;H01B3/44;

  • 国家 JP

  • 入库时间 2022-08-21 13:14:21

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号