PROBLEM TO BE SOLVED: To provide a repair material capable of handling a variety of small scale repair points such as cracks and holes, including micro pores generated in a road repair surface or water resistant layer, by improving fluidity to better poor viscosity during repair; and capable of preventing flash phenomena at high summer temperatures after construction, which exhibits impact resistance, viscoelasticity, plastic deformation, and the like, at an early stage, and which maintains an excellent condition for a long period of time.;SOLUTION: A repair material for pavement with fine powder is comprised of a mixture of 10-30 wt.% of a lubricant waste liquid or a lubricant, 0.5-3 wt.% of synthetic silica, 35-55 wt.% of blown asphalt having a penetration of 10-30, 12-30 wt.% of straight asphalt having a penetration of 100-200, 1-4 wt.% of rosin, 12-25 wt.% of slaked lime, and 1-6 wt.% of bentonite.;SELECTED DRAWING: None;COPYRIGHT: (C)2019,JPO&INPIT
机译:要解决的问题:通过改善流动性以改善修补过程中的较差粘度,提供一种能够处理各种小规模修补点的修补材料,例如裂缝和孔洞,包括道路修补表面或防水层中产生的微孔;并且能够防止在施工后的夏季高温下出现飞边现象,该现象在早期就表现出耐冲击性,粘弹性,塑性变形等,并且可以长期保持良好的状态。用细粉铺路的材料由以下混合物组成:10-30 wt。%的润滑剂废液或润滑剂,0.5-3 wt。%的合成硅石,35-55 wt。%的渗透性为渗透率为100-200的10-30、12-30 wt。%的纯沥青,1-4 wt。%的松香,12-25 wt。%的熟石灰和1-6 wt。%的膨润土。 ;选定的图纸:无;版权所有:(C)2019,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号