PROBLEM TO BE SOLVED: To provide a low-repulsive polyurethane foam capable of suppressing an increase in hardness in a low temperature region.;SOLUTION: A low-repulsive polyurethane foam is produced by an operation of reacting and foaming polyol which contains polyether polyol A having a molecular weight of 3,700-7,000, the number of functional groups of 2-4 and a hydroxyl value of 20-50 mgKOH/g, polyether polyol B having a molecular weight per the number of one functional group of 800-1,200, the number of functional groups of 2-3 and a hydroxyl value of 40-70 mgKOH/g so that a weight ratio of the polyol A to the polyol B is polyol A:polyol B=55:45 to 90:10, and MDI-based isocyanate while setting an isocyanate index at 60 to 115 in the presence of a foaming agent and a catalyst. The produced low-repulsive polyurethane foam F is provided on the surface of a sheet cushion 100 for vehicle.;SELECTED DRAWING: Figure 1;COPYRIGHT: (C)2018,JPO&INPIT
机译:解决的问题:提供一种能够抑制低温区域中硬度增加的低排斥性聚氨酯泡沫。解决方案:低排斥性聚氨酯泡沫是通过使含有聚醚多元醇A的多元醇发生反应并使其发泡而制得的分子量为3,700-7,000,官能团数为2-4,羟值为20-50 mgKOH / g的聚醚多元醇B,其分子量相对于一个官能团数为800-1,200,官能团的数目为2-3,羟基值为40-70 mgKOH / g,因此多元醇A与多元醇B的重量比为多元醇A:多元醇B = 55:45至90:10,而MDI-基异氰酸酯,同时在发泡剂和催化剂存在下将异氰酸酯指数设定为60至115。所生产的低排斥性聚氨酯泡沫F设置在车辆用片状缓冲垫100的表面上;选图:图1;版权所有:(C)2018,JPO&INPIT

著录项

  • 公开/公告号JP2018016748A

    专利类型

  • 公开/公告日2018-02-01

    原文格式PDF

  • 申请/专利权人 INOAC CORP;

    申请/专利号JP20160149487

  • 发明设计人 FUKAYA YUKIHIRO;

    申请日2016-07-29

  • 分类号C08G18/00;C08G18/48;C08G18/76;C08G101/00;

  • 国家 JP

  • 入库时间 2022-08-21 13:12:01

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号