首页> 外国专利> HETEROATOM-CONTAINING NANOCARBON MATERIAL, PREPARATION METHOD AND USE THEREOF, AND METHOD FOR DEHYDROGENATION REACTION OF HYDROCARBONS

HETEROATOM-CONTAINING NANOCARBON MATERIAL, PREPARATION METHOD AND USE THEREOF, AND METHOD FOR DEHYDROGENATION REACTION OF HYDROCARBONS

机译:含杂原子的纳米碳材料,制备方法和用途以及对烃进行脱氢反应的方法

摘要

A heteroatom-containing nano-carbon material, based on the total weight of said heteroatom-containing nano-carbon material and calculated as the elements, has an oxygen content of 1-6 wt %, a nitrogen content of 0-2 wt %, a carbon content of 92-99 wt %. In its XPS, the ratio of the oxygen content as determined with the peak(s) in the range of 531.0-532.5 eV to the oxygen content as determined with the peak(s) in the range of 532.6-533.5 eV is 0.2-0.8; the ratio of the carbon content as determined with the peak(s) in the range of 288.6-288.8 eV to the carbon content as determined with the peak(s) in the range of 286.0-286.2 eV is 0.2-1; the ratio of the nitrogen content as determined with the peak(s) in the range of 398.5-400.1 eV to the total nitrogen content is 0.7-1. The heteroatom-containing nano-carbon material shows a good catalytic capability in dehydrogenation of hydrocarbons.
机译:基于所述含杂原子的纳米碳材料的总重量并作为元素计算,所述含杂原子的纳米碳材料的氧含量为1-6重量%,氮含量为0-2重量%,碳含量为92-99重量%。在其XPS中,以531.0-532.5 eV范围内的一个峰确定的氧含量与以532.6-533.5 eV范围内的一个峰确定的氧含量之比为0.2-0.8 ;由在288.6-288.8eV范围内的一个峰确定的碳含量与在286.0-286.2eV范围内的一个峰确定的碳含量之比为0.2-1;由398.5-400.1 eV范围内的一个峰确定的氮含量与总氮含量之比为0.7-1。含杂原子的纳米碳材料在烃的脱氢中显示出良好的催化能力。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号