Process For Manufacturing Agglomerated Particles Of Tantalum, Mixed Tantalum Powder And Process For Manufacturing Same, Tantalum Pellet And Process For Manufacturing Same, And Capacitor

机译:钽,混合钽粉的凝集颗粒的制造方法及其制造方法,钽球及其制造方法和电容器

摘要

A method for producing agglomerated tantalum particles, comprising: a step for grinding secondary tantalum particles, which are obtained by reducing a tantalum salt, and adding water thereto to give a water-containing mass; a step for drying said water-containing mass to give a dry mass; a step for sieving said dry mass to give spherical particles; and a step for heating said spherical particles. A mixed tantalum powder comprising a mixture of agglomerated tantalum particles (X) with agglomerated tantalum particles (Y), wherein said agglomerated tantalum particles (X) show a cumulative percentage of particles with particle size of 3 μm or less of 5 mass % or less after 25 W ultrasonic radiation for 10 min, while said agglomerated tantalum particles (Y) show a cumulative percentage of particles with particle size of 3 μm or less of 10 mass % or more after 25 W ultrasonic radiation for 10 min.
机译:一种制造团聚钽颗粒的方法,该方法包括:研磨次级钽颗粒的步骤,该次级钽颗粒是通过还原钽盐并向其中添加水而获得的,从而得到含水的物质。将所述含水物料干燥以得到干燥物料的步骤;筛分所述干物质以得到球形颗粒的步骤;加热所述球形颗粒的步骤。混合钽粉,其包含钽凝聚粒子(X)和钽凝聚粒子(Y)的混合物,其中,所述钽凝聚粒子(X)的3μm以下的粒子的累积百分率为5质量%以下。在25 W超声辐射10分钟后,所述聚集的钽颗粒(Y)在25 W超声辐射10分钟后显示出3μm以下的粒径为10质量%以上的颗粒的累积百分比。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号