首页> 外国专利> ENVIRONMENTALLY FRIENDLY, NON-CLAY, AQUEOUS-BASED, BORATE CROSS-LINKER SLURRIES USING BORON-CONTAINING MINERALS

ENVIRONMENTALLY FRIENDLY, NON-CLAY, AQUEOUS-BASED, BORATE CROSS-LINKER SLURRIES USING BORON-CONTAINING MINERALS

机译:环保,含硼矿物的非黏土,水基硼酸盐交联剂浆液

摘要

Methods and compositions regarding borate, cross-linking suspensions are disclosed that may include one or more non-clay suspending agents, at least 30 wt. % of one or more boron-containing minerals, and a water-based solvent. In additional embodiments, the suspensions may include one or more polyols, one or more additives, or both, wherein the additives, for example, may include stabilizing agents, dispersing agents, surfactants, wetting agents, anti-gelling agents, pour-point depressants, or combinations thereof. Turning to a different aspect of this disclosure are methods that may include mixing one or more non-clay suspending agents in a water-based solvent and adding, subsequent to this mixing, at least 30 wt. % of one or more boron-containing minerals. In other embodiments, example methods may also include adding one or more additives prior to adding at least 30 wt. % of one or more boron-containing minerals.
机译:公开了关于硼酸盐,交联悬浮液的方法和组合物,其可以包含一种或多种至少30重量%的非粘土悬浮剂。 %的一种或多种含硼矿物和一种水基溶剂。在另外的实施方案中,悬浮液可包括一种或多种多元醇,一种或多种添加剂或两者,其中例如添加剂可包括稳定剂,分散剂,表面活性剂,湿润剂,抗凝胶剂,降凝剂。 ,或其组合。转向本公开内容的不同方面的方法可以包括将一种或多种非粘土悬浮剂在水基溶剂中混合,并且在该混合之后添加至少30重量%的非粘土悬浮剂。一种或多种含硼矿物的百分比。在其他实施方案中,示例性方法还可包括在添加至少30wt。%之前添加一种或多种添加剂。一种或多种含硼矿物的百分比。

著录项

  • 公开/公告号US2018258335A1

    专利类型

  • 公开/公告日2018-09-13

    原文格式PDF

  • 申请/专利权人 RADIXKHEM LLC;

    申请/专利号US201815976148

  • 发明设计人 MANJIT S. CHOWDHARY;

    申请日2018-05-10

  • 分类号C09K8/03;C09K8/88;C09K8/90;

  • 国家 US

  • 入库时间 2022-08-21 13:02:34