首页> 外国专利> CATALYST WITH A MESOPOROUS AND MACROPOROUS CO-MIXED NICKEL ACTIVE PHASE HAVING A MEDIAN MACROPORE DIAMETER IN THE RANGE 50 TO 300 NM, AND ITS USE IN HYDROGENATION

CATALYST WITH A MESOPOROUS AND MACROPOROUS CO-MIXED NICKEL ACTIVE PHASE HAVING A MEDIAN MACROPORE DIAMETER IN THE RANGE 50 TO 300 NM, AND ITS USE IN HYDROGENATION

机译:介孔和大孔共混镍活性相的中值大孔直径在50至300 NM之间的催化剂,及其在加氢中的用途

摘要

A catalyst comprising a calcined oxide matrix which is mainly alumina and an active phase comprising nickel, said active phase being at least partially co-mixed within said calcined oxide matrix which is mainly alumina, the nickel content being in the range 5% to 65% by weight of said element with respect to the total mass of catalyst, said active phase not comprising any metal from group VIB, the nickel particles having a diameter of less than 15 nm, said catalyst having a median mesopore diameter in the range 12 nm to 25 nm, a median macropore diameter in the range 50 to 300 nm, a mesopore volume, measured by mercury porosimetry, of 0.40 mL/g or more and a total pore volume, measured by mercury porosimetry, of 0.45 mL/g or more. The process for the preparation of said catalyst, and its use in a hydrogenation process.
机译:包含主要为氧化铝的煅烧氧化物基质和包含镍的活性相的催化剂,所述活性相在所述主要为氧化铝的煅烧氧化物基质中至少部分共混,镍含量为5%至65%相对于催化剂的总质量,以所述元素的重量计,所述活性相不包含VIB族的任何金属,镍颗粒的直径小于15nm,所述催化剂的中孔直径在12nm至5nm之间。 25nm,中值大孔直径在50至300nm范围内,通过水银孔隙率法测量的中孔体积为0.40mL / g或更高,并且通过水银孔隙率法测量的总孔体积为0.45mL / g或更高。所述催化剂的制备方法及其在氢化过程中的用途。

著录项

  • 公开/公告号US2018154340A1

    专利类型

  • 公开/公告日2018-06-07

    原文格式PDF

  • 申请/专利权人 IFP ENERGIES NOUVELLES;

    申请/专利号US201515317839

  • 申请日2015-06-09

  • 分类号B01J23/755;C07C5/03;C07C5/10;C07C5/05;C10G45/36;C10G45/48;B01J21/04;B01J35/10;B01J35/02;B01J37/08;B01J37/03;B01J37;B01J37/02;B01J37/04;

  • 国家 US

  • 入库时间 2022-08-21 13:01:41

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号